High Carbon Steel Wire Rod swrh82a

High strength and hardness

Cold processing

Fatigue strength and elasticity

Quality and size
| Element | Content range (%) | Core function |
|---|---|---|
| Carbon (C) | 0.79 - 0.86 | Core strengthening element, providing high strength and hardness |
| Silicon (Si) | 0.15 - 0.35 | Deoxidation, improving strength and elasticity |
| Manganese (Mn) | 0.30 - 0.60 | Improving hardenability, strength and wear resistance |
| Phosphorus (P) | ≤ 0.030 | Harmful elements, strictly controlled (the lower the better) |
|---|---|---|
| Sulfur (S) | ≤ 0.030 | Harmful elements, affecting hot brittleness (the lower the better) |
| Performance indicators | Typical value range/state description |
|---|---|
| Tensile strength (Rm) | ≈ 1080 MPa or higher (depending on size and state) |
| Reduction of area (Z) | ≥ 30% (good ductility) |
| Hardness (HV) | ≈ 320 - 380 HV (rolled/annealed reference) |
Application of SWRH82A wire rod

Why choose SWRH82A steel wire rod from us?
You Can Contact Us Here !
For inquiries about our products or pricelist, please leave your email to us and we will be in touch within 24 hours.
Quotation Questions ◢
-
Q.
What Chinese brand is SWRH82A equivalent to?
-
Q.
How to choose the "state" of the wire (such as rolled state, spheroidized annealed state)?
-
Q.
How can we ensure that SWRH82A can produce fasteners of grade 10.9 or 12.9?
-
Q.
Can you provide materials that meet specific corporate standards?
A.Absolutely! Our extensive steel mill resources enable us to meet the special technical requirements of different customers (such as tighter chemical composition range, lower inclusion level, specific decarburization depth requirements, special surface finish, etc.). Please provide your detailed standards or technical agreements.